In this research AA6060 alloy was used and was §extruded at 25m/min, 30m/min, 35m/min, 40m/min and§45m/min for a particular profile. The highest exit§temperature increased from 542°C to 567°C when the§extrusion speed was increased ... więcej

51.45

Zwykle: 52.51 €

Oszczędzasz 1.06 €


Dostępna u dostawcy
Wysyłamy za 15 - 20 dni
Dodaj do schowka

Zobacz książki o podobnej tematyce

Podaruj tę książkę jeszcze dziś
  1. Zamów książkę i wybierz "Wyślij jako prezent".
  2. Natychmiast wyślemy Ci bon podarunkowy, który możesz przekazać adresatowi prezentu.
  3. Książka zostanie wysłana do adresata, a Ty o nic nie musisz się martwić.

Dowiedz się więcej

Więcej informacji o Effects of Extrusion Process Conditions on Die Pick-Up

Za ten zakup dostaniesz 131 punkty

Opis

In this research AA6060 alloy was used and was §extruded at 25m/min, 30m/min, 35m/min, 40m/min and§45m/min for a particular profile. The highest exit§temperature increased from 542°C to 567°C when the§extrusion speed was increased from 25m/min to 45m/min.§Three types of die pick-up were identified. They were§named as normal pick-up, die line pick-up and lump§pick-up. Normal pick-up occurred regardless of the§extrusion speed and exit temperature; however the§amount of normal pick-up did not increase when the§extrusion speed was increased. Die line pick-up §occurred when the extrusion speed was 45m/min and§appeared only on the die lines. Lump pick-up is not§significant since it was very rare.§AA6060 (0.4%Mg and 0.5%Si) alloy has about 0.27% §excess silicon and therefore at 555°C, Mg2Si§particles react with aluminium and excess silicon to§form liquid. However normal pick-up and die line§pick-up still occurred at temperatures lower and§higher than 555°C and therefore it confirms that§eutectic reactions do not influence formation of pickup.§Therefore die pick-up is most likely to be caused §due to a mechanical process rather§than a metallurgical process.

Szczegóły książki

Kategoria Książki po angielsku Mathematics & science Physics

51.45

Ulubione w innej kategorii



Osobní odběr Bratislava a 2642 dalších

Copyright ©2008-24 najlacnejsie-knihy.sk Wszelkie prawa zastrzeżonePrywatnieCookies


Konto: Logowanie
Všetky knihy sveta na jednom mieste. Navyše za skvelé ceny.

Nákupní košík ( prázdný )

Nakupte za 59,99 € a
máte doručení zdarma.

Twoja lokalizacja: