Kód: 17353171
This handbook was produced with the intention of providing failure analysts who work with spaceflight metals a reference of SEM fractographs of fracture surfaces produced under known conditions. The metals and the fracture conditi ... celý popis
20.57 €
Bežne: 21.01 €
Ušetríte 0.44 €
Nákupom získate 52 bodov
This handbook was produced with the intention of providing failure analysts who work with spaceflight metals a reference of SEM fractographs of fracture surfaces produced under known conditions. The metals and the fracture conditions were chosen to simulat